Microstructures and Energy Storage Properties of Sr0.5Ba0.5Nb2O6 Ceramics with BaO-B2O3-SiO2 Glass A

来源 :第七届中国储能与动力电池及其关键材料学术研讨与技术交流会 | 被引量 : 0次 | 上传用户:pearljeejee
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
  Sr0.5Ba0.5Nb2O6(SBN)ceramics with the BaO-B2O3-SiO2(BBS)glasses have been successfully produced for high energy-storage density capacitor applications.
其他文献
In this paper,we report a template-free method to fabricate hollow nitrogen-doped carbon(HNC) by pyrolysis of hollow polyaniline(PANI) microspheres,which were synthesized by suspension polymerization
会议
随着便携式电子产品和电动汽车的发展,超级电容器和充电电池已经成为了2种非常重要的储能方式.其中超级电容器因其优良的功率密度和长期的循环性能而广受关注.
会议
The electrochemical characteristics of a redox couple and the transport properties of corresponding ions in the DES determine the availability of this redox couple in non-aqueous flow batteries.
会议
We would like to introduce the self-assembly of MnO2 nanostructures with controllable morphology for electrochemical supercapacitor,including mesoporous MnO2 nanotubes and their arrays,carbon-MnO2 coa
会议
Rechargeable Na-ion battery has attracted lots of attention in recent years due to its huge availability of sodium,low price and the similarity of both Li and Na insertion chemistries1,2.In this work,
会议
In this work,we made an attempt to use FEC as an electrolyte additive to improve the high voltage stability of LiCoO2/Li battery.The use of dimethyl methylphosphonate(DMMP) as a flame-retardant additi
会议
It has been reported that TNT has enormous potential as photo-catalysts because of their peculiar properties which originate from their low dimensionality.
会议
目前锂离子电池已经广泛用于移动电子设备,人造卫星和航空航天等领域,也是混合电动汽车和纯电动汽车的重要选择。 传统的商业化锂离子电池正极材料LiMnO2,LiCoO2和LiFePO4的理论比容量都低于170 mAh g-1,这使得电池的能量密度很难有大的提升。
会议
The porous carbons have been prepared by chemical activation using commercial activated carbons as precursors and KOH as the chemical agent, and the MnO2 and MnO2-loaded porous carbons have been synth
本实验通过模板法直接水热合成了有序介孔Fe-N/C材料,具有简单、经济和可持续的特点.试验中采用三聚氨胶硫酸盐控制碳源与软模板的有机自组装过程,引入硫酸铁为碳源,一步水热合成铁修饰的有序介孔氮掺杂碳材料.
会议