One of the major challenges in spot welding of ultra-thin gage steel (e.g., < 0.6ram) is the short cap life.Because of the elevated temperature developed at
Titanium and its alloys are well known as the typical different-to-cut material because of their low thermal conductivity, high chemical reactivity and low