论文部分内容阅读
The Np-Pu simulated solution was concentrated and transformed by using microwave concentration method.The solids obtained from microwave concentration were calcinated in order to achieve simulated radioactive incineration ash (SRIA).Zirconolite (CaZrYi2O7) was used to contain the SRIA with different containments.