发展铁酸钙进一步改善高铁低硅高碱度烧结矿质量

来源 :武钢技术 | 被引量 : 0次 | 上传用户:zhanghai_007
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
一、前言精料是高炉强化冶炼、实现高产优质低耗的物质基础。烧结矿在炉料中占主要地位,因此改善烧结矿的质量就成为“精料”的主要内容。近年来,国内外都十分重视提高烧结矿的品位,以利高炉节焦增铁。随着钢铁工业的发展,选矿技术的进步,我国的精矿品位在不断提高,由原全铁含量62~63%提高到67~68%,为提高烧结矿含铁品位提供了有利条件,使烧结矿的全铁含量由过去的50%左右提高到54~55%,为高炉精料作出了贡献。 First, the preamble Concentrate is the blast furnace to strengthen smelting, to achieve the material basis of high yield, high quality and low consumption. Sinter plays a major role in charging materials, so improving the quality of sinter becomes the main content of “concentrate”. In recent years, both at home and abroad attach great importance to improving the quality of sinter, to facilitate blast furnace section coke by iron. With the development of the iron and steel industry and the progress of beneficiation technology, the grade of concentrate in our country is continuously improving, increasing from 62-63% of the original total iron content to 67-68%, providing favorable conditions for improving the iron content in sinter, The total iron content of sinter increased from about 50% in the past to 54-55%, contributing to blast furnace concentrate.
其他文献
测定了碱度(CaO/SiO[*v2*])在1.54~2.53范围内的烧结矿的高温(1200℃)还原性。结果表明,碱度为1.85~1.91的烧结矿的高温还原性比其它的好,同时FeO含量愈低,还原性愈高。试用未反应
该文阐明了高架轻轨交通的环境影响因素,影响分析方法及该市拟建浦东轻轨、莘闵轻轨及南北快速交通轨道工程的环境影响,并提出了可行的环保对策建议。
生产高碱度小球团烧结矿,配加生石灰作为熔剂和粘结剂,造成5~10mm的小球团,放置30min,小球团的自粉率很低。小球团烧结指标较高。
在一定的条件下,高硅低铁高碱度烧结矿是增铁节焦的一条有效途径,在大量实验研究的基础上,分析了高硅低铁高碱度烧结矿还原性差的根本原因,提出了改善这种烧结矿还原性的措施