Drying kinetics study of irregular fibril materials in a “differential” laboratory rotary dryer:Case

来源 :中国烟草学会2018年学术年会 | 被引量 : 0次 | 上传用户:sddhyyj
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
  Rotary dryers are commonly used in the modern large-scale tobacco drying industry that consumes huge amounts of energy.In fact,rotary dryers are commonly used in chemical industry in general.It is difficult to investigate the drying behavior at industrial scale.A “differential” laboratory rotary dryer was therefore designed and tested.The large diameter of the industrial dryer was preserved,but the width was a section of the industrial dryer.The drying characteristics of cut tobacco from top leaves and bottom leaves with initial moisture contents(22.5±1.0%on the wet basis)were studied in the “differential” dryer at air temperatures of 65,85,105,125,and 145℃,respectively.The results show that increasing drying temperature accelerated the drying process,whereas the surface temperatures of the cut tobacco samples stayed in the temperature range of 48–71℃ when their moisture contents were reduced to 12.0±1.0%(wb).This 12.0%(wb)was required by commercial operations.Uniquely,the drying kinetics was captured using the reaction engineering approach(REA).Although different settings were applied,the model can be used to describe all the data well.The unique relationship between the normalized activation energy and the moisture content is approximated which is independent of the drying air temperature and the tobacco origin.The different drying behaviors for the cut tobacco from top leaves and bottom leaves can be attributed to their different equilibrium isotherms.Through controlling the drying time as predicted by REA model,the outlet moisture contents of cut tobacco from top leaves dried at 95℃/RH0.034/320 s and 115℃/RH0.017/250 s were shown to be 12.3 and 11.8%(wb),with the relative deviations of 2.5 and 1.7%,respectively,and these were within the industrial permissible range.
其他文献
本文介绍了一种替换传统测量水样氢电导率(需经过阳离子交换树脂柱)的智能型氢电导率仪表,由于该仪表不需要更换或再生树脂,所以真正意义上实现了氢电导率的连续在线准确测量。智能型氢电导率仪表在凝汽器检漏装置上的应用,可以在测量数据无干扰的情况下准确迅速反映凝结水品质的变化,对准确判断凝汽器是否泄漏和泄漏位置起了关键的作用。
分析了我厂2×600MW超临界机组实施锅炉给水加氧处理项目的背景、决策过程和实施效果。针对国内现有的多种加氧处理技术和加氧装置,通过大量调查研究最终确定采用全保护加氧处理工艺和设备。应用结果表明,全保护加氧处理技术和装置是解决超(超)临界机组水汽系统腐蚀、结垢,提高机组运行经济性的最为安全、可靠的加氧处理方法。
针对某电厂两台600MW直流炉水汽指标异常问题进行了分析,通过对可能引起水汽品质异常的原因进行排查,并对各水汽取样点进行TOC/TOCi、痕量离子含量、氢电导率综合分析,确定了引起水汽指标异常的主要原因。
针对某650MW超临界机组汽轮机高压缸调速级及主汽高调门阀芯集中积盐问题进行现场调查和原因分析,并将本次机组运行工况与上次大修期间机组运行工况和积盐情况进行对比,发现深度调峰对超临界机组积盐规律存在影响。
300MW机组运行时,出现水汽指标中氢电导率严重超标,同时伴随凝结水精处理高速混床迅速失效等问题。从锅炉补给水处理系统着手分析,研究发现问题的“元凶”是大量尿素泄漏进入锅炉补给水处理系统,通过除盐水进入锅炉热力系统所致。
文中通过基体金属腐蚀部位形貌和腐蚀产物检测,结合机组运行状况针对某联合循环机组给水加药管道腐蚀失效原因进行了分析。给水加药管道腐蚀失效原因分析结论对联合循环机组给水加药的运行管理和加药管道选材提供了一种经验。
通过查找、分析凝结水溶解氧超标的原因,实施了密封系统改造、轴封回水管、凝汽器补水管安装位置等工艺优化,降低了凝结水溶解氧含量,减轻了溶解氧腐蚀,提高了水汽系统的合格率。
EDTA在较低温度下溶解性较差。而低温EDTA化学清洗技术需要在较低温度下对EDTA进行溶解。因此EDTA加药方式对清洗结果会产生至关重要的影响。本文阐述了三种不同的低温EDTA加药方式,通过对比三种方式和实际验证得出清洗泵循环加药方式是最为理想的选择,并对此方法进行了优化。
会议