论文部分内容阅读
A coating of composition Si-40Mo (wt pct) was prepared by fused slurry coating method on the two-dimensional carbon/carbon (2D-C/C) composite to improve oxidation resistance. In the procedure of the fabrication, pure Si slurry inner layer in the pre-coati