分析了阳极炭块氧化掉渣和裂纹掉块的危害 ,并按危害程序予以分类 ,根据我国实际情况指出四个主要影响因素 ;原料质量、骨料细度等配料工艺条件、焙烧工艺和电解槽技术条件。
According to the hazardous process, four main influencing factors were pointed out: raw material quality, fineness of aggregate and other ingredients, roasting process and electrolyzer Technical conditions.