论文部分内容阅读
开发了60t钢包炉喂Al线,Ti芯线和B芯线工艺.实践结果表明,Al的平均回收率为78.0%.Ti为92.7%.B为85.0%。
Developed 60t ladle furnace feeding Al wire, Ti core wire and B core wire craft. The practice results show that the average recovery of Al is 78.0%. Ti is 92.7%. B is 85.0%.