【摘 要】
:
自行车车架钎焊前清洗(即化学除油),对钎焊质量有很大影响。钎焊后尽管各工序按照工艺进行,但检查后,仍发现少量车架有开焊现象。试验发现,开焊的车架是由于钎焊前没有彻底
论文部分内容阅读
自行车车架钎焊前清洗(即化学除油),对钎焊质量有很大影响。钎焊后尽管各工序按照工艺进行,但检查后,仍发现少量车架有开焊现象。试验发现,开焊的车架是由于钎焊前没有彻底清除油污所致。目前一些厂使用的清洗液配方大同小异。据多次试验,发现这些配方只能去掉管子上较少的油污,油污程度稍微严重,便无能为力。在实践中,找到了一种新的配方:即,氢
Brazing before the bicycle frame cleaning (ie chemical degreasing), the quality of the brazing has a great impact. Despite the brazing process in accordance with the process, but after inspection, still found a small amount of frame has a welding phenomenon. The test found that the welded frame is due to the brazing did not completely remove the oil before. Some of the current factory cleaning fluid formulations are similar. According to several tests, it has been found that these formulations can only remove less oil on the pipelines, and the degree of oiliness is a little serious and powerless. In practice, a new formula has been found: hydrogen
其他文献
北京师范学院恒源电火花机床厂与机械工业部、北京机床研究所共同研制的SLC—120B型脉冲电源,于1982年10月底通过技术鉴定。该电源是用于电火花成型机床的大功率节能脉冲电
把市场机制引入公共资源配置、公共资产交易、公共产品生产领域,积极推进以市场为取向的“三公”领域改革,对于进一步完善社会主义市场经济体制,促进政府职能转变、维护社会
青山湖区塘山镇青湖村村党支部书记、村委会主任万少荣和“一班人”一道,坚持真抓实干,不断改革创新,积极引领党员干部群众在思想上适应大机遇、能力上驾驭大发展、作风上保
目前,冷轧管机的工艺利用系数是0.75~0.85。若送进卡盘的返回和轧辊对管坯的压下结合进行,作业时间则能得到充分利用。这样,在每一个轧制周期里必须完成管坯的夹紧、送进、回
A high-speed and high-res ol ution optical A/D quantizer is proposed. Its architecture is discussed. Bit circ uits are built by using the phase modulators in pa
The photochemical isomerization of trans and cis-difluorostilbenes has been studied.In the presence of a photosensitizer (biacetyl, 0.05 mol·L~(-1)) about 75%
In structural chemistry,it has been well accepted that,besides orbital interactions,geo-metrical factors e.g.size and shape of the bonded atoms and groups,may
在国内首先引用放射性同位素法,快速得出了刀具耐用度与切削速度的关系。精确地查明了切削过程中刀具磨损进展的模型。
In the first reference to radioisotope method, qu
钛及钛合金具有比重小、强度大、耐高温、抗腐蚀等优异性能,已成为有色冶金工业有前途的结构材料之一。苏联有色冶金工业部门每年大约生产2300吨钛设备和钛部件。其中,北方
可靠性是衡量产品质量和经济效益的重要指标,一般以无故障间隔时间越长,产品失效率越短,则其可靠性越高。影响产品可靠性的因素,可能有设计思想上的,也有使用方面的。尽管目