通过10万吨钢的工业性试验表明,将低碳镇静钢帽容比由10.5%降互9.5%后,成坯率提高0.87%钢质量符合现行标准要求,工艺可行,经济效益明显。
The industrial test of 100000 tons of steel shows that the quality of low carbon steel can be improved by 0.87% after 10.5% reduction from 9.5% to 9.5%, the quality of steel meets the current standard, the technology is feasible and the economic benefit is obvious.