论文部分内容阅读
Cubic boron nitride(CBN) micro powders and mixture of CBN micro powders with Al or Ti powders were fast heated at 1 300,1 400,1 450,1 500℃,and then kept for 5 min under spark plasma sintering (SPS).The obtained powders were analyzed with XRD.The results s