论文部分内容阅读
Fe-6.5wt%Si composite compact was fabricated by spark plasma sintering(SPS).Mechanical alloying(MA)was used to prepare Fe-Si composite powders.The composite powders were sintered by SPS at elevsated temperature from 500℃ to 700℃.The experimental results indicate that the non-equilibrium state of composite Fe-Si is preserved in the compact.The density of the bulk rises with the increasing temperature and there is no diffusion of silicon and iron in the interface.