Acid leaching solution was obtained after mixing pyrite cinders with H2SO4, then heating the mixture of pyrite cinders and H2SO4 at 200-300 ℃, leaching the hea
<正>The NiAl-28Cr-5.85Mo-0.15Hf alloy was prepared by high-pressure die casting (HPDC) and subsequent hot isostatic pressing(HIP), and tested for compressible s
The development of cube texture({001}<100>)in high purity(99.99%)aluminum foils in multistage annealing was investigated by ODF and EBSD.It is found that a mult