论文部分内容阅读
Nanosized amorphous TiO2 powders with a specific surface area of 501 m2.g-1 were prepared by hydrolysis. Aftercalcined at 400℃ for 2 h, the prepared amorphous TiO2 powders were fully transformed into anatase crystallitesthe samples of nanosized amorphous