This paper presents a reactive ion exchange synthesis method of nano-CeO2 with positive cerium preexchanged ion exchange resin as precursor and ( NH4) 2CO3 as precipitant. The resultant precipitate was dried at 100 ℃ for 12 h and then was calcined at 500