论文部分内容阅读
应用电镜及X射线衍射技术研究了含Cr及不含Cr的Fe-28at.-%Al合金中相变结果表明,1080℃淬火过程中,B2结构热畴已开始形成;缓冷通过B2相区,沿晶界出现α相;对Fe-28Al-5Cr合金还出现细小的CrN相沉淀,板状合金中B2→D03是一缓慢转变过程.
The Cr-containing and Cr-free Fe-28at were studied by means of electron microscopy and X-ray diffraction. -% Al alloy shows that during the quenching process at 1080 ℃, the thermal domain of B2 structure has begun to form; slow cooling passes through the B2 phase region and α phase appears along the grain boundary; fine CrN also appears in the Fe-28Al-5Cr alloy Phase precipitation, plate alloy B2 → D03 is a slow process of change.