介绍了纳米复合镀层制备技术存在的问题,综述了纳米复合镀层强化技术的现状,重点分析了液相等离子体强化技术的原理和分类。利用高能量密度的液相等离子体将镀件与基体加热到熔凝状态,使得镀层材料与基体材料相互渗透,形成再结晶组织,实现了两者的冶金结合,提高了镀层与基体的结合强度。 The problems existing in preparation technology of nanocomposite coatings were introduced. The current status of nanocomposite coatings strengthening technology was reviewed. The principle and classification of liquid phase plasma enhanced technologies were analyzed emphatically. The liquid phase plasma with high energy density heats the plating and the substrate to the fused state, so that the plating material and the matrix material penetrate each other to form a recrystallized structure, thereby achieving metallurgical bonding between the two and increasing the bonding strength between the plated layer and the substrate .
其他文献
目的 研究自拟参芪通络汤对缺血性中风患者脑保护机制.方法 将236例气虚血瘀兼水湿停滞型缺血性中风患者随机分为治疗组和对照组(治疗组116例、对照组117例).对照组予临床基
采用库仑滴定法测定铁矿石中的硫含量 ,利用智能测硫仪 ,在催化剂作用下 ,使铁矿石中的硫在高温下以SO2 形式释放出来 ,用电解生成的碘滴定H2 SO3,该方法准确度好 ,测量范围
期刊
现行国家标准规定:尿氟(班前≤4 mg/g肌酐;班末≤7 mg/g肌酐),均采用肌酐来界定尿中氟的生物限值.而现有的尿氟检测标准WS/T 30-1996中却是以尿液实际比重来换算标准比重下的
经冷轧变形和中间退火制备了Cu-15Cr形变原位纤维增强复合薄板材料。用SEM、拉伸试验机和电阻率测试仪研究了变形量及退火温度对Cr纤维形貌、合金强度及导电性能的影响。结果
国家经贸委发布了《“九五”国家重点技术开发指南》。《指南》是以市场需求或具有潜在市场为出发点 ,选择了市场前景好 ,技术先进 ,综合经济效益好 ,符合国家产业政策 ,对国
有毒中药用于临床时应否炮制?这个问题《神农本草经》的序言说得很清楚:"药有有毒无毒","若有毒宜制"。《内经》上的"治半夏",《伤寒论》中"附子炮""半夏洗",都说明制用的意义。由于历史
期刊
根据国家计划和市场需要 ,“九五”和 2 0 1 0年非金属矿产勘查主要任务和战略布署 :①加强金刚石、宝玉石等贵重矿产的勘查 ,增加储量 ;②加强农用矿物原料的勘查工作 ,注重
介绍了下挂式多级脉冲增效射孔和外套式多级脉冲增效射孔技术的作用原理、产品特点及技术指标.该设计采用了火工品中的隔板点火技术与延时技术,并对增效药剂的综合性能进行改