炭粉焙烧铝电解槽较焦炭焙烧可节约大量冶金焦及电力、减轻工人劳动强度及适应不需清槽和生产以后增建电解槽的焙烧要求。按我厂实际情况,确定将水银整流器总体化成与电解槽焙烧结合起来,按阳极铸型、通电焙烧、电解槽启动的步骤进行。铸型前作好设备、原材料准备。铸型要求槽膛必须清扫吹净,垫炭粉4公分厚,将阳极框架调整到距阴极槽底250毫
Charcoal roasting compared with coke roasting aluminum coke can save a lot of metallurgical coke and electricity, reduce labor intensity and adapt to do not need to clear the tank and production after the roasting requirements of the additional electrolyzer. According to the actual situation in our factory, it is determined that the mercury rectifier is integrated into the roasting together with the electrolyzer, and the steps are performed according to the anode mold, the power roasting and the electrolyzer start. Make equipment before mold, raw material preparation. Mold requirements must be clean the mouth of the groove blowing, charcoal powder 4 cm thick, the anode frame is adjusted to 250 milliliters from the bottom of the cathode