日前,江苏沙钢棒材生产线实现了∮16三切分新工艺调试全线贯通。该工艺的成功运行标志着沙钢在切分工艺技术水平上又大大向前迈进了一步。该棒材生产线系实现棒材生产线∮16三切分新工艺的调试运行,此套工艺相比于原来的三切分,有着显著的优势。原来的三切分在生产过程中故障比较多,尤其在切分过程中经常导致各线条形之间尺寸的不均匀的缺陷。该缺陷的存在一直是棒材多线切分生产工艺中的一个难点。传统多切分生产中,为了使得切分能够尽可能的均匀和稳定,通常在导卫上积极采取措施,在预切
Recently, Jiangsu Shagang bar production line to achieve ∮ 16 three cutting new technology debugging across the board. The successful operation of this process marks a significant step forward for Shagang in cutting the technological level of the process. The bar production line to achieve bar production line ∮ 16 three cutting new technology debugging operation, this set of technology compared to the original three points, has a significant advantage. The original three points in the production process more faults, especially in the segmentation process often leads to uneven dimensions between the lines of the defects. The existence of this defect has been a difficult point in the multi-strand bar production process. In the traditional multi-cutting production, in order to make the segmentation as uniform and stable as possible, we usually take the initiative to guide the guide on the pre-cut