Average grain size of chemicalty synthesized CePO4 powder increases with incre asing calcining temperature. The strength 184 Mpa and toughness 4.8 Mpa*m1/ 2 were achieved when the green compacts were sintered at 1500 ℃ for 2 h in air . They show that step