论文部分内容阅读
针对水钴矿制备钴盐生产过程中含锰、铜、钴、锌等重金属离子废水,通过4步除杂、P204萃取富集锰,制备电池材料用硫酸锰。第1步用硫化钠去除铜、钴、锌离子,硫化钠最佳加入量为60 g/L ;第2步用碳酸氢铵调pH去除铝,最佳pH为4.5;第3步用硫酸钠去除Ca2+,硫酸钠最佳用量为110 g/L ;第4步用氟化钠进一步去除Al3+和Ca2+,氟化钠最佳用量为0.45 g/L。4步除杂后的废水用P204萃取、硫酸反萃取,得到硫酸锰溶液,硫酸锰溶液经蒸发结晶得到电池材料用硫酸锰。“,”In the process of preparing of cobalt salt using heterogenite ,the wastewater which contains heavy metal ions such as M n2+ ,Cu2+ ,Co2+ ,Zn2+ was produced .By four-stages purification and solvent extracting ,manganese sulfate which could be applied in battery materials was obtained .In the first stage ,Cu2+ ,Co2+ ,Zn2+ are precipitated by sodium sulphide ,the optimum amounts of sodium sulphide is 60 g/L .In the second stage ,ammonium bicarbonate is used to adjust pH for hydrolytic precipitation aluminum .In the third stage ,sodium sulphate is used to remove Ca2+ ,the ideal amounts of sodium sulphate is 110 g/L .In the fourth stage ,Al3+ ,Ca2+ can be further purified by adding sodium fluoride , the best amount of sodium fluoride is 0 .45 g/L .After the above four steps ,manganese sulfate was obtained by P204-extraction and H2 SO4 anti-extraction ,evaporation and crystallization ,manganese sulfate used as battery materials can be obtained .