论文部分内容阅读
本文总结了钽—10%钨合金板材制取的熔炼加工工艺。叙述了最终尺寸为9×230×430毫米热轧板材和最终尺寸为1.5×200×300毫米冷轧板材的加工工艺参数。合金的成份及主要性能符合国际文献报导的标准。此项研究工作于七一年三月开始止于七一年十二月。
This article summarizes the tantalum-10% tungsten alloy plate prepared by the melting process. Described the final size of 9 × 230 × 430 mm hot-rolled sheet and the final size of 1.5 × 200 × 300 mm cold-rolled sheet processing parameters. Alloy composition and main performance in line with international standards reported in the literature. The study began in March 1973 and ended in December, December.