锤杆寿命与热处理

来源 :锻压机械 | 被引量 : 0次 | 上传用户:joeworms
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
锤杆受力情况复杂,应力变化剧烈,在工作时容易折断.我厂的一台5t锤每年平均要折断5根锤杆.为了提高锤杆的使用寿命,我们分析了锤杆折断的原因,在材质和热处理工艺两方面着手改进,收到了令人满意的效果.一、分析1.锤杆的材质用35CrMo替代40Cr作为锤杆的材料,不仅使锤杆具备了铬钢的抗蚀性和热稳定性,而且提高了锤杆热强度和降低了热脆的敏感性.2.锤杆的热处理 Hammer rod force situation is complicated, the stress changes drastically, easily broken at work.A 5t hammer of our plant averagely breaks 5 hammer rods every year.In order to improve the service life of the hammer rod, we analyzed the reason of hammer rod breakage, In the material and heat treatment process to improve both, received satisfactory results.A analysis 1. Hammer rod material used as a replacement for 40Cr hammer rod material 35CrMo, not only to make the hammer rod with chromium steel corrosion resistance and Thermal stability, but also improve the hot rod strength and reduce the sensitivity of the hot brittle .2 hammer rod heat treatment
其他文献
数控车床的加工质量与工艺装备、程编水平和操作经验等因素有密切相关。本文就数控车削中的工件尺寸控制问题谈些我们的做法。 一、轴向尺寸的控制 轴向尺寸可分两类:一类是
一、前言 本文对纯铅中As、Sn的分机 进行了条件选择,试验方法适于铅分类中1、2、3号铅中的As、Sn分析,本方法还可推广应用于铅中Zn、Sb的分析。 大家知道,纯铅中As、Sn的含
研究了45钢Fe_2B硼化层经激光熔化处理熔池深度和激光参数之间的关系及临界熔化层中的相分布,发现:(1)在给定的激光功率密度下,熔池深度H与扫描速度v有如下关系:H=K/v~(0.65)
影视艺术教育在全国高校蓬勃发展,辽宁省对高校影视艺术教育的发展也很重视,许多高校开设了影视艺术专业。文章从辽宁省高校影视艺术教育的现状入手,分析辽宁省影视艺术教育
我厂在自制导轨磨床时,采用长3m的C650型普通车床(图1)解决了导轨磨床身(图2)端面加工问题。我们先考虑了以下几点: 1.工件的一端应能用四爪卡盘装夹,另一端能够可靠使用顶尖
某电厂工程,根据美国土建设计要求,采用ASTM Grade—60钢筋。为节省外汇,电厂拟采用性能和Grade—60钢筋相接近的国产25MnSiⅢ级钢筋替代,其机械性能见表。根据美国ASTM标准
根据长期生产φ1200、φ1500球磨机巴氏合金球面轴瓦和其他轴瓦的经验,将浇注巴氏合金球面轴瓦所常见的缺陷及其焊补办法介绍于下: 一、缺陷 1.裂纹:常出现在轴承合金层表面
解放后,随着社会主义建设事业的发展,在沙漠地区修建了多条干线公路,对巩固国防,繁荣城乡经济,以及开发沙漠地区的自然资源起到重要作用,但是,由于沙漠地区气候干燥少雨、风
我厂开发研制的DY型精密端齿分度盘在1988年中国机床工具博览会优秀展品“春燕奖”的评比中获得了“春燕奖”二等奖、银牌(外观见本期封面)。该分度盘能帮助用户在50年代的机
插齿刀工作时的产形齿轮齿廓是切削刃在端面上的投影,由于前后角的影响,这个投影不是渐开线,故被切齿轮便产生了齿形误差。误差值随前后角的增大而增大;误差方向随前角的正负