论文部分内容阅读
SiC porous ceramics were prepared at 1 400 ℃ for4 h with crystalline silicon cutting waste and activated carbon as main starting materials and NH4HCO3 as the pore-forming agent. Effects of NH4HCO3 additions( 0,20%,30%,40%,by mass) on the phase composition