5.3.5萤光粉应用 现在叙述光学塗复制造萤光粉点屏即使用的方法。新近革新的黑色阴模屏,放在5.5节叙述。第一步,用一种基色萤光粉混合物,塗复玻璃面板内部屏衬底表面,一种有机粘合剂。如用水稀释的乙烯醇,和一种(?)光胶敏化剂,通常是胺化合物,用机器使面板倾斜旋转,当混合物由中心进入后,就扩展到边缘,然后,旋转机器,使面板与垂直位置成一适合角度,以清除多余塗料,当面板萤光粉层干燥时,就成为光敏的。这时应放在黄色安全光处。
5.3.5 Phosphor Applications Now that the optical coating manufacturing phosphor screen is used. The newly redesigned black matrix screen, described in Section 5.5. The first step, using a base color phosphor mixture, coats the interior surface of the glass panel interior substrate, an organic binder. Such as water-diluted vinyl alcohol, and a (?) Light-sensitive sensitizer, usually an amine compound, are used to tilt the panel with the machine and spread to the edges as the mixture enters the center, and then the machine is turned so that the panel An appropriate angle to the vertical to clear excess paint, the panel becomes light-sensitive when the phosphor layer is dry. This time should be placed in yellow safety light.