The modification of silica coating surfaces by trimethylsilylation has contributed to enhanced hydrophobicity (θow>90°) against fluid permeation and corrosion
The combined effect of pre-aging and Ag/Cu addition on natural aging and bake hardening in Al-Mg-Si alloys were studied by Vickers microhardness measurement, te
SiC ceramic has been successfully joined to Zr4 alloy using TiZrNiCu filler within the temperature range 1173 K-1263 K and 15 min holding time. The morphology o
Microarc oxidation (MAO) electrolysis plasma deposition was used to prepare Al2O3 coatings on Ti-45Al-8.5 Nb alloys to improve high temperature oxidation resist
The properties of nickel-base superalloy pipes are determined by microstructure, and the microstructure can be tuned by hot extrusion process. There are two maj