稀土氟碳酸盐矿物的拉曼光谱研究

来源 :光谱学与光谱分析 | 被引量 : 0次 | 上传用户:asdfghjka
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
研究了氟碳钡铈矿Ce2Ba[CO3]3F2、氟碳钙铈矿Ce2Ca[CO3]3F2和氟碳铈矿Ce[CO3]2F等矿物的拉曼光谱特征。结果表明,钡稀土氟碳酸盐矿物(氟碳钡铈矿、氟碳铈钡矿、黄河矿)的Raman光谱特点是,ν1和ν2为单峰值,ν3和ν4为双峰值。钙稀土氟碳酸盐矿物(氟碳钙铈矿)的拉曼光谱带中ν1和ν4为双峰值,ν2和ν3为单峰值。稀土氟碳酸盐矿物(氟碳铈矿)的Raman光谱的特点是,ν1、ν2和ν4为单峰值,ν3为双峰值。 The Raman spectra of Ce2Ba [CO3] 3F2, Ce2Ca [CO3] 3F2 and Ce [CO3] 2F from bastnaesite were studied. The results show that Raman spectra of barium-bearing rare earth fluorocarbon minerals (bastnaesite, bastnaesite and yellow river) are that ν1 and ν2 are single peaks and ν3 and ν4 are bimodals. In the Raman spectrum of the calcium-rare-earth fluorocarbon mineral (bastnaesite), ν1 and ν4 are bimodal, and ν2 and ν3 are unimodal. The Raman spectrum of rare earth fluorocarbon minerals (bastnaesite) is characterized by ν1, ν2 and ν4 as single peaks and ν3 as bimodal peaks.
其他文献
本文通过盐酸普鲁卡因的紫外光谱,确定了盐酸普鲁卡因两种型体(分子型体和离子型体)存在时的pH值,并研究了这两种型体加入β-环糊精、HP-β-环糊精和Methyl-β-环糊精前后荧光强度的变化。 In t
由于极端气候事件频发,洪水灾害发生频率和影响越来越大,人们对灾害的研究从关注致灾因子转移到易损性,并认为易损性是灾害的根本原因.作者在分析现有易损性研究基础上,从系
本文叙述了吸光度比值-导数光谱新方法的原理,研究了在普通分光光度计上用计算法完成吸光度比值导数运算、同时测定苯酚和间苯二酚含量的实验方法,取得了较为满意的结果。苯酚的
本文提出了用ICP-AES法测定马口铁中的痕量铅。试样用NaOH-H2O2溶解镀层。测得四种样品的含铅量在0.14~0.38μg/cm2范围内。方法的回收率为96.1%~103.2%。方法的精密度(RSD)为2.6%~3.8%。本法简便迅速,测量结果的准确度、精密度满足分析
利用红外光谱,核磁共振波谱对一种未知化合物的结构进行了研究分析,证明是酞酰苯胺酸。这对研究该物质的生物活性及生化机理将十分有益。 The structure of an unknown compou
本文通过对二硝基氯苯与吡啶生成的紫红色化合物光谱的研究,从而导出了主次双波长对二硝基氯苯进行定量测定的数学模型,二硝基氯苯在0~50 μg/25 mL范围内计算参数(Y)与二硝基
钨盐涂覆处理石墨管,大幅度提高测定锂的灵敏度。配以(NH4)2SO4基体改进剂,消除生物基体干扰。特征浓度5.53×10-3μg·mL-1/1%,回收率大于93.72%,相对标准偏差小于8.93%。 Tungsten-coated graphite tubes significa
用FT-Raman光谱研究了在不同浓度的氘代甲醇-重水溶液中溶菌酶的构象。结果表明,随着氘代甲醇浓度的增加,溶菌酶结构逐渐松散,并形成凝胶。松散β-折叠结构增多是产生凝胶的原因。 The co
本文在电镀沉积的银衬底上,研究了硫脲分子在酸性溶液中的表面增强拉曼散射。结果表明,硫脲分子是通过硫原子倾斜着吸附在银表面;当溶液中的HCl浓度增加时,在银表面吸附的硫脲分子面