预制圆形混凝土柱的缺陷及防治

来源 :建筑工人 | 被引量 : 0次 | 上传用户:kaokao514
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
预制圆形混凝土柱时,拆模后表面常出现气孔、麻面、露筋、微细裂纹等缺陷。例如我们制作某工程冷却塔人字柱时,施工初期就遇到人字柱表面有气孔现象,后经不断改进,才克服了这种缺陷。一、施工概况及遇到的问题该人字柱长9.67m,截面直径为0.65m,竖向钢筋为18φ25,螺旋箍筋为φ10@200,混凝土强度等级为C30、P6、F150,该冷却塔共有人字柱88根。预制地点设在工地预制场内。模板为上、下两个半圆扣合模具,由10 When prefabricated circular concrete columns are used, defects such as pores, hemp surfaces, exposed tendons, and fine cracks often appear on the surface after the mold is removed. For example, when we made a cooling tower column for an engineering project, we encountered stomatal phenomena on the surface of the herringbone during the initial period of construction. After continuous improvement, we overcome this defect. I. Construction Overview and Problems Encountered The length of the post is 9.67m, the section diameter is 0.65m, the vertical reinforcement is 18φ25, the spiral stirrup is φ10@200, and the concrete strength grade is C30, P6, F150. The cooling tower A total of 88 people columns. The prefabrication site is located in the site prefabrication field. The template is the upper and lower two semi-circular fastening dies, which are composed of 10
其他文献
期刊
上虞之所以能跻身全国百强县之列,建筑业功不可没!rn贡献一:为地方财政提供了重要收入来源rn近年来,上虞建筑业一直保持着强劲发展势头,与此同时,全市建筑业税收也呈现了稳健
在工业与民用建筑中,水泥砂浆地面应用最广泛,但如果使用材料不当、施工方法不规范,就容易产生裂纹、起砂、脱皮、麻面和空鼓等质量通病。笔者根据工作经验及探索,就如何避
期刊
黄河石,中华观赏石百花园中一朵靓丽的奇葩。人们收藏她、观赏她、赞美她。她的亮点究竟在哪里?笔者在赏石实践中认识到,黄河石具有鲜明的特性和独特的优势。黄河生成。母亲
期刊
《信息自由法》是美国宪政制度的重要组成部分,在这部法律的制订和完善过程中,美国传媒起到了积极的推动作用。出台后的信息自由法,成为传媒获取政府信息、监督政府权力的途
学位
拉斯维加斯(Las Vegas)地处美国内华达州被荒凉的沙漠和半沙漠地带包围的山谷地区,30年代,内华达州决定使赌博成为合法的事业,此令一出,几乎在一夜之间,赌场纷纷成立,拉斯维
互联网正以山呼海啸的态势向报纸等传统媒介施压。互联网以及依托其形态的新媒体已经超过报纸、广播、电视等传统三大媒体,成为第四媒体。目前中国以互联网为代表的新媒体事
期刊