长期以来,灰铸铁的生产水平比较低,生产较高牌号的灰铸铁常采用低,碳当量的方法,铸件废品率较高。实践使我们认识到,高温铁水、高废钢配料、高碳当量是获得优质高强度灰铸铁的重要前提。我们通过提高灰铸铁的硅碳比以改善铸件质量、提高材质的性能。经过较长时间的试验生产,取得了满意的结果。现将低应力高强度优质灰铸铁在中型铣床上的试验及生产应用情况总结如下,以供参考。一、化学成分及生产试验条件 For a long time, the production level of gray iron is relatively low. Gray iron with higher grades often adopts low and carbon equivalent methods, resulting in a higher reject rate of castings. Practice has made us realize that high-temperature hot metal, high-scrap ingredients, high carbon equivalent is an important prerequisite for obtaining high-quality, high-strength gray cast iron. We improve the quality of castings by improving the silicon-carbon ratio of gray cast iron. After a long period of trial production, and achieved satisfactory results. Now the low-stress high-strength high-quality gray cast iron in medium-sized milling machine test and production applications are summarized below for reference. First, the chemical composition and production test conditions
其他文献
+一、管子上半圆搭接角焊缝(一)焊前准备1.试管的加工选用φ159×6mm的20钢管,切割成长250mm的半圆管,然后用砂轮机将搭接部位磨修平整。试管尺寸见图5-1。2.试管的清理试管
我厂产品上的关键件,脱落插头是酚醛玻璃纤维压塑料和磷青铜的组合件.由于酚醛玻璃纤维压塑料电解除油时(温度为80°C),塑料表面亮膜遭到腐蚀后失去光泽变黑.以前我厂一直采
热处理的能耗一般为成本的15%,机械制造业的热处理一般占其用电总量的40%,因此尽快采用节能技术,加强科学管理,实现节能高产十分必要。本文就五金制造方面的热处理节能途径提
东方红75拖拉机行走机构台车的调整垫片(见图1)厚度分别为0.2、0.4、0.6mm,年需要量达几十万件。根据生产批量大的要求,我厂将J 23-60t压床加上一套自动进退料机构组成自动
我公司承担了宁波农药厂杀螟工程,其中两台浓硝酸贮坛(下图),由20mm厚的纯铝板(L2),采用双面同步手工钨极氩弧焊焊接而成,较好地解决了厚铝板的焊接技术。 Our company und
近年来,企业流动资金紧张,供血不足,血液循环不畅,原因是多方面的。但从较长的时间跨度来看,我们认为,根本原因是积累构成不合理,积累内部比例失调,固定资产积累比重过高,流
GN1-1包缝机下刀(图1),材料为T10A,该零件小而薄,极易弯曲变形。我们过去采用低碳钢专用夹具成串压紧,在盐浴炉于790~800℃加热8~10min后,在盐水中淬火冷却(图2)。这个淬火工
钢中加入微量钙可提高钢的加工性能,但微量钙的分析尚无合适方法.1985年钢铁系统为了制订和考核钢中钙、镁的原子吸收分析法,组织了十多个单位进行试验和考核.考核证明,本方
1、适用范围 本标准规定了;铜、铝、铅、锡合金的轧制和铸造坯料,采用机械加工和坯料成形方法制造的滑动整体轴承合金材料的硬度检验。 本标准是对ISO现有的关于硬度检验标
近代技术的发展对钨、铝中杂质元素的分析灵敏度和准确度提出了愈来愈高的要求,促使分析工作者不断地完善分析方法,而载体分镏法是分析纯钨、钼中微量杂质元素的主要方法。