论文部分内容阅读
利用作者试验室合成的捕收剂采用离子浮选法进行了钨钼分离.对于(NH4)2WO4溶液和Na2WO4溶液体系,每克钼捕收剂用量为676g的条件下,对于含钼量为04~12g/L的料液,其除钼率可达到94%~99%.
The tungsten and molybdenum separation was carried out by ion flotation using the collector synthesized by the author laboratory. For (NH4) 2WO4 solution and Na2WO4 solution system, the dosage of molybdenum per gram of catalyst is 676g, the removal rate of molybdenum can reach to 04 ~ 12g / L 94% ~ 99%.