论文部分内容阅读
Curie temperature of amorphous alloys Co_(90-x)Cr_x Zr_(10) decreases linearly with increas-ing x.Average magnetic moment per magnetic atom Co or Cr is 1.51 μB or -3.62 μBrespectively.The temperature dependence of spontaneous magnetization at low temper-atures is in agreement with Bloch’s T~(3/2) law.The spin wave stiffness constant decreaseswith increasing x from 4 to 20.The range of interaction is 2—3 atoms for x=4 andnearest neighbour atom for x=20.The crystallization temperature increases mono-tonically with increasing x.It may relate to the average number of outer electrons peratom.The crystalline phase components of heat-treated alloys were analyzed by X-raydiffration and thermomagnetic measurement.
Curie temperature of amorphous alloys Co_ (90-x) Cr_x Zr_ (10) decreases linearly with increas-ing x.Average magnetic moment per magnetic atom Co or Cr is 1.51 μB or -3.62 μBrespectively.The temperature dependence of spontaneous magnetization at low temper -atures is in agreement with Bloch’s T ~ (3/2) law. The spin wave stiffness constant decreases with increasing x from 4 to 20. The range of interactions is 2-3 atoms for x = 4 and neighbors atom atom for x = 20. The crystallization temperature increases mono-tonically with increasing x.It may relate to the average number of outer electrons peratom. The crystalline phase components of heat-treated alloys were analyzed by X-raydiffration and thermomagnetic measurement.