The miscibility of the blend,composed of a bisphenol A epoxy resins (Diglycidyl etherof bisphenol A) (DGEBA) and poly(ethylene oxide) (PEO) and crosslinked by p
Ladderlike polychloropropylsilsesquioxane (CP-T) was first synthesized by 'stepwise coupling polymerization'.The molecular weight of CP-T is as high as
The sol/gel phase diagrams were studied for two systems: polyacrylamide/Cr (III) andpolyacrylamide/glyoxal. Sol or gel phase could be distinguished according to