论文部分内容阅读
1977年以来,我们采用国产弹性印模衬料,-SDL-1-43型室温硫化甲基硅橡胶(以下简称室温胶),作为复制总义齿的涂衬材料。取得了较好的效果。疗效观察五年多来,我们为25例患者(男18,女7)复制了上、下颌总义齿共41件。计上颌总义齿24件:包括树酯牙列15件,金属(牙合)面牙列9件;下颌总义齿17件:包括树酯牙列12件,金属(牙合)面牙列5件。随访病人18例(男13,女5)。该18例患者具有上、下总义齿共28件,其中金属(牙合)面牙列及树酯牙列各14件。病人一致反映咀嚼功能好,可与第一副交换使用,戴在口中无异感。随访戴用树酯
Since 1977, we have adopted the domestic elastic impression lining material, -SDL-1-43 room temperature vulcanized methyl silicone rubber (hereinafter referred to as room temperature glue), as a copy of the denture coating material. Achieved good results. For more than five years, we have performed a total of 41 upper and lower total dentures on 25 patients (18 male and 7 female). Total maxillary total denture 24: Including the resin dentition column 15, the metal occlusal dentition column 9; Mandibular total denture 17: Including the resin dentition 12, the metal occlusal dentition 5 . 18 patients (male 13, female 5) were followed up. The 18 patients had total upper and lower total denture 28, of which metal (occlusal) surface dentition and resin dentition each 14. Uniform reflection of patients with good chewing function, with the first exchange of use, wearing the same no sense of the mouth. Followed wearing resin