The effect of minor additions of Sn on the as-cast ageing behavior of Al-11Si-0.35Mg alloy was investigated. It is shown that precipitation has been retarded in
Cavitation erosion behavior of nickel-aluminum bronze(NAB)weldment in 3.5% NaCl aqueous solution was studied by magnetostrictive vibratory device for cavitation