Crystallisation kinetic and phase transformation behaviour of the electroless nicke l-phosphorus deposit with 6-9wt% phosphorus content were studied. The deposit washeated in the differential scanning calorimetry (DSC) apparatus to 300℃ 800℃ at20℃/rain,