论文部分内容阅读
分析了涂料自身材料质量、温度影响、施工速度因素和施划后受外力作用等而产生不同形状、不同程度的开裂原因,并提出减少标线开裂、提高标线质量的几点观点。
Analysis of the paint material itself, the impact of temperature, construction speed factor and the external force after the application of different shapes, different degrees of cracking reasons, and put forward to reduce the line marking cracking, marking several points to improve quality.