The plates of AA5086 aluminium alloy were joined together by friction stir welding at a fixed rotation speed of 1000 r/min various welding speeds ranging from 63 to 100 mm/min.Corrosion behavior of the parent alloy(PA),the heat affected zone(HAZ),and the