西钢高炉扩容改造后,通过采取一系列强化冶炼措施,使两座高炉利用系数长期稳定在3.1t/(m~3·d)以上,最高达3.5t/(m~3·d)。本文介绍了西钢采取的主要措施。
After the expansion of the blast furnace in Xihua Iron and Steel Co., Ltd., a series of intensification smelting measures have been adopted to make the utilization coefficient of both blast furnaces stable over the long term range from 3.1 t / (m ~ 3 · d) up to 3.5 t / (m ~ 3 · d). This article describes the West Steel to take the main measures.