自行车上涂底漆,多数使用156黑色打底漆及头度黑烘漆,采用浸、浇、淋的工艺方法,结果漆膜厚度不匀,在边角尖端和缝隙处涂不上,防锈能力差,且容易产生流疤(疙瘩)、砂粒及不平整等缺陷。我厂职工在党的领导下,和上海染料涂料研究所、振华造漆厂等单位的协助下,打破框框,发扬敢想敢说敢为的革命精神,经过200多次的试验,终于试验成功电泳涂化新工艺,摸索了一些电泳涂化的规律,并对部
Bicycle primer, the majority of the use of 156 black primer and black degree of black paint, the use of immersion, pouring, pouring process, the results of uneven film thickness, at the corner of the tip and gap coating, rust Poor ability, and prone to flow scar (pimples), sand and uneven defects. Under the leadership of the party and with the assistance of the Shanghai Institute of Dyeing and Coatings, Zhenhua Paint Factory and other units, our factory workers break the framework and carry forward the revolutionary spirit of daring to say and say. After more than 200 trials, they finally experimented Successful electrophoresis Tuhua new technology, explore some of the rules of electrophoretic coating, and the Department