Hardness of the TiB2/7075 composite increased with increasing deformation temperature. In the annealed TiB2/7075 composite, a great amount of fiber-like MgZn2 phases (about 1 μm in length) and small MgZn2 phases (about 100 nm in size) were precipitated ne