论文部分内容阅读
1996年世界炼钢技术要闻1.世界首家采用Corex法的南非伊斯科公司比勒陀利亚厂电炉用Corex铁水作炉料,生产率提高60%。该厂采用高达50%的平均含碳4.5%的Corex铁水为炉料,熔炼速率为72t/h,而采用100%的废钢炉料仅为45t/h。...
World steelmaking technology news in 1996 1. The world’s first Corex hot-blast furnace in Pretoria, South Africa, using the Corex method, produced 60% more productivity. The plant uses up to 50% Corex hot metal with an average carbon content of 4.5% for a feed rate of 72 t / h compared to 45 t / h for 100% scrap steel. ...