燃油气锅炉多为卧式内燃锅壳锅炉。该种锅炉的结构特点及制造使用过程中的缺陷,是导致其管板裂纹的主要原因。现就该型锅炉制造使用环节提出几点看法。
Most of the gas-fired boilers are horizontal internal combustion boiler shell boilers. The structure of the boiler and manufacturing process defects, is the main reason leading to the crack of the tube plate. Now on the type of boiler manufacturing links made a few comments.