天井吊盘掘进試驗初步總結

来源 :有色金属(冶炼部分) | 被引量 : 0次 | 上传用户:shellyyiqiong
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
采用吊盘掘进天井是高效率的掘进方法。1955年在苏联某矿采用此法掘进天井,最高日进尺达到6.6米,平均日进尺达4.7米的水平。为此,今年2月分,某矿务局与长沙矿山設計院共同进行了这一試验,其結果証实了:能达到速度快,节省木材,改善劳动条件。現将試驗情况介绍如下: 一、試驗条件天井的高度(岩石厚度)为20.8米,断面4平方米(2×2米)所穿过的岩石为大理石及鉛鋅夹黄铁 The use of hanging plate for tunneling is an efficient method of excavation. In 1955, a mine in the Soviet Union used this method to excavate patios. The maximum daily footage reached 6.6 meters and the average daily footage reached 4.7 meters. To this end, in February this year, a mining bureau and Changsha Mining Design Institute conducted a joint test, the results confirmed: to achieve speed, save wood, improve working conditions. Now the test conditions are described below: First, the test conditions Patio height (rock thickness) of 20.8 meters, 4 square meters section (2 × 2 meters) through the rocks for the marble and lead-zinc clip yellow iron
其他文献
平炉钢炉后脱硫的方法——平炉钢炉后脱硫的原理——镇静钢的炉后脱硫——沸腾钢的炉后脱硫——硅钢的炉后脱硫——讨论——炉后脱硫的钢的质量——新脱硫剂的探讨 Method f
为了达到既筛除烧结矿粉末,同时减轻粉尘污染的目的,重钢炼铁厂经实验研究后,于1980年在620米~3高炉槽下建成风力筛分热烧结矿系统. 由该系统筛分后,烧结矿粉末含量由15~25%
攸县人民钢铁厂投入生产的四座高炉的有效容积为58.5m~3。高炉附属设备简陋,机器陈旧,100(?)发电机组已使用40余年,特别是风机能力还满足不了生产要求,除三号高炉配有两个27
Four kinds of assays were used to study the effect of a fat-soluble extract of spinach powder (SPFE) on the proliferation of human gastric adenocareinoma cell l
小高炉炉顶调节的意义和目的——装料制度的选择——寻求合理的CO_2曲线——用炉顶调节来调节炉况 The Significance and Purpose of Small Blast Furnace Top Adjustment -
技术操作方法:(1)在实际操作中,使用人工接钎,首先将六角空心钢钎断头处,用夹甜放入墟中,烧红以后,扩大中心孔,再使用鎚子敲扁打尖。一般的打尖坡角,大约在15°~20°左右。(2
对燒結在生产实踐过程中所要求的是:燒結良好,塊銅硫比一定,塊率高生产力大,坚硬多孔合乎熔爐理想造渣成份的自熔性燒結塊。为了达到这些目的,我們在燒結实际生产中对下面几
关于煉鋅鼓風爐的發展过程中的一些工作情况,已經在其他的地方談过了,現在我們想談一下关于阿旺茅斯商業規模爐子操作过程中的一些成就,特别着重于爐子与冷凝器的一些因素及
唐山钢厂的大型氧气站已于去年建成。第一炼鋼車間的转爐目前已全部使用富氧鼓风。平均富氧程度为25%左右。生产实践表明转爐富氧吹炼的效果是: 1.縮短了鼓风时間約10%; 2.铁
太原钢铁公司第二炼钢厂在今年6月份首先试验成功了侧吹碱性转炉不烘炉炼钢.目前这个先进经验不仅在该厂全面推广,而且已经为上海、北京、重庆等地许多转炉钢厂所采用。但是