论文部分内容阅读
Dense ceramic oxide coatings of about 50 μm may be prepared on Ti-6Al-4V alloy surface by alternating-currentmicroarc oxidation in aluminate and silicate solutions, respectively. Their phase constituent and microstructure werecharacterized using X-ray dif