[期刊论文] 作者:QIAN Yuejin,YU Xingguo,JIANG M,
来源:中国耐火材料:英文版 年份:2012
Cr2O3 can be sintered well at 1 500 ℃ in carbon-embedded condition or H2 atmosphere. But the high chrome bearing refractories can not reach densification when...
[期刊论文] 作者:QIAN Yuejin,JIANG Mingxue,LI L,
来源:中国耐火材料:英文版 年份:2009
Pure Cr2O3 refractories and high Cr2O3 bearing refractories are difficult to sinter in oxidizing atmosphere,but they can be sintered easily in carbon embedded c...
Effect of Atmosphere on Sintering of High Cr2O3 Bearing Refractories Considered from Thermodynamic C
[期刊论文] 作者:QIAN Yuejin,JIANG Mingxue,LI L,
来源:中国耐火材料 年份:2004
Pure Cr2O3 refractories and high Cr2O3 bearing refractories are difficult to sinter in oxidizing atmosphere, but they can be sintered easily in carbon embedded...