Fundamental Process of Iron Acetate Synthesis for the Recovery of Neodymium Magnet

来源 :The 12th International Symposium on East Asian Recycling Tec | 被引量 : 0次 | 上传用户:whsdht
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
  Iron(Ⅲ)acetate was synthesized for recycling of neodymium magnet.Iron is main element in acidic leaching solution of neodymium magnet.Iron acetate is a basic material for synthesizing iron nanoparticles and catalyst for synthesizing carbon nanotube.
其他文献
  Bioleaching provides an alternative for inexpensive,low-energy consumption and being environmentally safe for metal extraction from low grade-ores or scraps
  Extraction processes of cobalt from cobalt mineral ore are divided into pyrometallurgical and hydrometallurgical process.
  In this paper,the low-grade zinc oxide ore of high alkaline-gangue was treated through cycle leaching method in NH4Cl-NH3-H2O system(namely MACA system).
  In the process of production of solar wafers,about 30-40%silicon raw material powder will lost with grinding slurry in the warp cutting procedure.
  Low temperature alkaline smelting(LTAS)is an effective cleaner product method in non-ferrous metallurgy,especially in the separation and extraction of compl
  The traditional zinc hydrometallurgy process produce a large number of iron-based slags,which also contains a small amount of zinc,copper,indium,germanium a
  Recently,amount of waste solution containing gold is increasing according to the growth of electric and electronic industry.
  In pyrometallurgical production process of some nonferrous metal,such as copper and nickle,a large quantity of slag with high ferrum content is produced.How
  Kitakyushu city,which is located in the north part of Kyushu,has an industrial activity on the environment.Its a long history to overcome the public nuisanc
  The recovery of copper from electric furnace slag through the deep cleaning smelting process is studied.The physical properties of the slag are improved fir