【摘 要】
:
The water environment of pressurized water reactor is high pressure and high temperature,meanwhile,in order to protect steam generators,the water chemistry in the secondary loop of PWR is required to
【机 构】
:
Keyscience new Technology Beijing ltd
【出 处】
:
第三届核电厂材料与安全可靠性国际研讨会 (3rd MRNPP Symposium)
论文部分内容阅读
The water environment of pressurized water reactor is high pressure and high temperature,meanwhile,in order to protect steam generators,the water chemistry in the secondary loop of PWR is required to be high in pH and low in dissolved oxygen(DO).However,under this water chemistry condition,the carbon steel piping of secondary loop is prone to flow accelerated corrosion(FAC),a corrosion mechanism in which a normally protective oxide layer on a metal surface dissolves in fast flowing water,and underlying metal corrodes to recreate the oxide,and thus the metal loss continues.The purpose of this paper is to build a device which can simulate the secondary loop of PWR.The device has the required velocity,temperature and pressure,and can control the pH,DO and other parameters.It can be used to study the effect of pH,DO and velocity of FAC.The corrosion data of carbon steel in PWR secondary loop can be obtained from this device.
其他文献
The commercial Alloy 690TT was first immersed in the normal hydrogenated primary water at 325 ℃ and 15.6 MPa for 720h and then immersed in the oxygenated primary water at 325℃ and 15.6 MPa for 720h wi
Steam generation tubing materials have the susceptibility of stress corrosion cracking(SCC)under the severe steam conditions.Alloy 600,Alloy 800 and Alloy 690 are widely used as the steam generation t
The stress corrosion cracking(SCC)behavior f A508/52M part in dissimilar metal weld A508/52M/316L in simulated primary water environments at 290℃ was investigated by means of slow strain rate testing(
The effect of strain rate on stress corrosion cracking of 316LN SS in borated and lithiated(B/Li)high temperature water was studied.The results showed that SCC occurred only in a certain strain rate r
In this paper we studied the effects of temperature and dissolved oxygen on crack growth rate in 316L type stainless steel used as auxiliary pipe in nuclear power systems in high purity water under th
The crack growth rates(CGRs)of a domestic forged nuclear grade 316L SS piping material were measured at various temperatures and loading modes in simulated pressurized water reactor primary water envi
Characterizations of the microstructure and chemical composition of oxide films formed on 316NG stainless steel following exposure experiments in high temperature water with various dissolved hydrogen
Stress corrosion cracking(SCC)of sensitized 304 stainless steel(SS)in borated and lithiated high temperature water without and with Zn injection was studied using slow stain rate test(SSRT)and surface
This paper introduces a new test model and data acquisition plan for evaluation of materials of thin-walled tubes of nuclear power plant.In analogy to crack growth rate measurements using compact tens
The microstructure and distribution of residual strains were investigated in the fusion boundary region of domestic low alloy steel SA-508Ⅲ weld joint using scanning electron microscope(SEM),electron