用缺口冲击韧性作为评定铝焊接构件的判据

来源 :国外舰船技术(材料类) | 被引量 : 0次 | 上传用户:yush2000
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
一、近况介绍变形铝合金用于受压容器时,其基体材料和焊接接头的屈服强度、抗拉强度、伸长率、弯曲角、硬度和缺口冲击韧性等的最低值均应根据BV30—9/74[1]加以验证。屈服强度、抗拉强度和伸长率之数值系在拉伸试验中确定,并表征材料在单向载荷下的性能。缺口冲击韧性的测定用于评定材料的韧性和脆性断裂的倾向。这个与文献相符的 First, the current situation Introduction Deformation aluminum alloy used in pressure vessels, the base material and welded joints yield strength, tensile strength, elongation, bending angle, hardness and notch impact toughness, etc. should be based on BV30-9 / 74 [1] to verify. The values ​​of yield strength, tensile strength and elongation are determined in the tensile test and characterize the material under uniaxial load. The notched impact toughness is used to assess the tenacity of the material and the tendency of the brittle fracture. This is consistent with the literature
其他文献
连续流动快原子轰击质谱法(Continuous Flow Fast Atom Bombardment Mass Spectrometry, CF-FABMS)采用连续流动进样技术将样品溶液不断地引进离子源,经快原子轰击电离、质
318无缝钢管车间是在60年代建成的,采用皮尔格轧管机轧制钢管,钢管定径为五辊定径机,定径前再加热是用端部进料,侧面出料的斜底式加热炉。80年初将斜底炉改为步进梁式加热炉
大家知道,表面质量是指零件加工后表面光洁度、表面层显微组织变形硬化、残余应力、烧伤及裂纹等问题,研究表面质量的目的,主要是控制零件的加工表面质量,以延长零件的使用寿
2009年12月14日~19日,中国引航协会组织了首个赴台考察团,对台湾引航机构发展与组织管理进行考察。考察团先后拜访了台湾引水人联合会,基隆、花莲、高雄、台中四个港口及当地
八、氮化炉的管系装置 (1)管件材料──由於氨对许多金属如锌、铅、铝、黄铜、白铁等有腐蚀性(尤以铜类为甚),因此在整个的氮化管系中,所用的管件、管子阀和接头等最好用镍铬
一、定义所谓高Cr铸铁,就是含Cr10%以上的铸铁。其上限一般为32%,比这再高,无论在文献上还是在实践中都不实用。(Si+Al)在3%以下时,由于高Cr铸铁在组织中不含石墨,全部成白
本文用含稀土化合物的钛系催化剂(代号SN-1)于乙烯与苯乙烯的共聚反应进行了研究.讨论了单体比例、催化剂浓度、Al/Ti的摩尔比和反应温度对共聚合的影响.制备出苯乙烯链节含
本文公式及表格较多,整理时因时间关系未能一一核对,内中可能有些地方计算错误,希读者注意,如发现有错误,请与本刊联系,以便更正。——编者 丝锥为制造螺母或螺丝孔的刃具,其
本世纪五十年代以来,二过碘酸合铜(Ⅲ)和二过碲酸合铜(Ⅲ)配离子作为氧化剂在糖类、氨基酸。蛋白质、羧酸和醇类等的定量测定中得到了广泛的应用。近期Movius和Murthy等人进
熔铸锆莫来石耐火砖、是以高铝矾土、工业氧化铝粉、锆英砂及少量的熔剂Na_2O、CaO;按照一定的化学组成,进行配料计算(配合料应具有适宜的颗粒组成)并经过混合、成型、干燥