V、Nb和Ta元素对高铬铸铁结晶与铸态组织的影响

来源 :兵器材料科学与工程 | 被引量 : 0次 | 上传用户:sheena111
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
高铬铸铁广泛地应用于磨料介质中工作的铸件。高铬铸铁县有很高的耐磨性,首先是由于其组织中存在有大量的含铬碳化合物。碳当量CE为4.2~4.3%的合金具有最好的耐磨性,在此种合金中,含有数量最多的分枝状共晶碳化物Cr_7C_3继续提高碳和铬的合金化时,在组织中将会出现粗大、针状的铬的一次碳化物。使其与金属基体的联系削弱,因而会急剧降低高铬铸铁的机械性能和耐磨性。此种情况阻碍了高铬铸铁依靠 High-chromium cast iron is widely used in abrasive media work castings. High chromium cast iron county has a high wear resistance, first of all due to the presence of a large number of chromium-containing carbon compounds in its organization. The alloy with carbon equivalent CE of 4.2 ~ 4.3% has the best wear resistance. In the alloy containing the largest amount of branched eutectic carbide Cr_7C_3, when the alloying of carbon and chromium continues to be improved, There will be coarse, needle-shaped primary carbides. Weakened its connection with the metal matrix, which drastically reduced the mechanical properties and wear resistance of high chromium cast iron. This situation hindered the high-chromium cast iron from relying
其他文献
本文较系统地论述了金属的喷丸强化与组织、性能之间的关系,并指出了当前喷丸工艺中的问题是弹丸的技术要求和喷丸的饱和时间。 This paper systematically discusses the r
本文研究了热循环的改变对焊接热影响区冲击韧性的影响及其断口特征。实验结果说明,冷速越大,冲击韧性越好;冷却时间长,显微组织粗化,出现粗大孪晶马氏体,这是影响韧性低的主
高锰钢在较大冲击或接触应力作用下,表面会迅速产生加工硬化形成高硬度、高耐磨的表面层,而内层仍然保持良好的冲击韧性。即使零件磨损到很薄,仍能承受较大的冲击载荷而不致
东非包括肯尼亚、乌干达和坦桑尼亚三国,地处赤道两侧,大致在北纬4°至南纬10°东径20°~40°之间,面积约175万平方公里,人口5000多万。高原地形的大部分在海拔1000米以上。
姦淫谋殺,几成为美国在西德兵的家常便饭。最近即有四个美国兵,与德国居民发生一连串衝突,其中並包括强姦和谋害人命的暴行。美军负责人承认说已有两个士兵自首说他们是谋殺
传统磷化液是用氧化锌(ZnO)、硝酸(HNO_3)、磷酸(H_3PO_4)、水(H_2O)按一定重量比例配制而成。配制时,浓硝酸挥发出二氧化氮(NO_2)黄烟,对配料工人身体健康有严重危害,同时
一、问题的提出在用X射线衍射法测定钢中残余奥氏体含量时,一般都沿用Cohen方法来处理,其结果是以残余奥氏体含量的体积百分数V_A表示 V_A=(1-V_c)/(1+G_M~A(I_M/I_A) (1)式
以正确的设计计算方法选用滚动轴承,使曲轴支承滚动轴承化,效率提高至0.6以上,行程速度按需要成十倍地提高,轴承寿命达到或超过机器的大修周期,工作扭矩减少1/6,电机功率缩小
图1是一个90t钢锭锻造成直径1500mm时距底部端1200mm(全长4800mm)以内部分纵断面的宏观组织照片。假如把其中五个缺陷的位置还原到钢锭上,它们都处在直径100~150mm范围内并距
一、前言铝合金型材表面的“白斑套黑点”腐蚀斑点(图1)是一种什么性质的缺陷?斑点区的非金属物,如Ca、S、Cl等是否是基体金属中的夹杂物?本文通过电子探针和电镜分析查明: