论文部分内容阅读
江西省萍乡钢铁厂于1964年3月在一座容积100米~3高炉上采用流槽冲渣法获得了成功。通过十个月的生产实践,证明了这种方法是可行的。目前日产水渣为70—80吨。流槽冲渣的工艺流程如图: 在放渣前一分钟左右启动水泵6,将蓄水池7的水打入流槽5。当高炉出渣时(上渣或下渣),从渣口(或铁口)出来的熔渣流入流槽5,遇到流量很大的高压水发生急剧的水淬作用,使熔渣冲制成散粒状的细渣,在流槽中被急流的水冲到较远的沉渣滤水池9沉积下来,滤水后,
Pingxiang Iron and Steel Plant in Jiangxi Province in March 1964 in a volume of 100 to 3 blast furnace slag flow method using slag success. After ten months of production practice, this method is proved to be feasible. Nissan current slag is 70-80 tons. Flow tank dregs process shown in Figure: Put the slag in the first minute or so before starting the pump 6, the reservoir 7 water into the runner 5. When the blast furnace slag (on the slag or slag), from the slag mouth (or iron mouth) out of the slag flow into the flow channel 5 encountered a very large flow of high-pressure water rapid quenching water, slag making Into the granular granular slag, the rapids in the rapids rushed to the far sediment sedimentation tank 9 deposition, water filtration,